A tubular heater is a sealed metal tube with MgO inside. If the end weld leaks, moisture gets into the MgO, insulation drops, and the element grounds out.
Welding methods
- TIG (argon arc) welding: clean, full penetration, standard for industrial heaters
- Brazing with brass: cheaper, but brass corrodes in wet environments, do not use for immersion
- Resistance welding: thin walls only, not for high pressure
What we check after welding
- Leak test under 0.5 MPa air pressure in water bath - no bubbles
- Insulation resistance above 500 M ohm after 24 hours humidity
- Visual: no pinholes, no burn-through
A customer bought cheap tubular heaters from a trader. They looked the same but failed in 3 months in a water tank. We cut one open - the end cap was brazed, and water had crept along the joint. TIG welded units run 5 years in the same tank.
Need TIG-welded tubular heaters?
Tell us the sheath material and application. We TIG weld every end.
Send Your Specs