A customer sent back a batch of tubular heaters that kept burning out near the bend. We found the fabricator had bent the 10mm tube to a 10mm radius - basically folding it in half. That cracked the MgO insulation and shorted the resistance wire.
The rule we follow
- 6mm tube: minimum bend radius 1.5xD = 9mm
- 8mm tube: minimum bend radius 1.5xD = 12mm
- 10mm tube: minimum bend radius 1.5xD = 15mm
- 12mm tube: minimum bend radius 2xD = 24mm
Below that radius, the internal resistance wire kinks and the compacted MgO cracks. The heater may work when new, but it fails within weeks from vibration or thermal cycling.
What if you need a tighter bend?
We can use a smaller diameter tube with higher wattage to achieve the same total power in a tighter space. Or use a formed cast heater. Do not just bend the tube tighter and hope.
If your drawing calls for a bend radius smaller than the tube diameter, send it to us first. We will tell you if it is buildable or suggest an alternative.
Need custom bent tubular heaters?
Send us your drawing. We will check the bend radii and quote accordingly.
Send Drawing