TIG Welding Stainless Steel Tubular Heaters: Why Argon Matters

Every tubular heater has one critical weld: the end cap where the lead wires exit. If that weld leaks, moisture gets into the MgO powder and the element grounds out.

Why TIG, not MIG

TIG (GTAW) uses a tungsten electrode and pure argon shield. The weld pool is tiny and controlled. On a 10 mm diameter stainless tube with 1 mm wall, you need to melt the end cap without blowing through the tube.

MIG (GMAW) is faster but the wire feed is harder to control on thin wall. It burns through 1 mm tube easily. Brazing uses brass filler - brass corrodes in wet environments and the joint is not hermetic.

Parameters we use

Backing gas

On 316L and Incoloy welds, we purge the inside with argon. Without backing gas, the inside of the weld oxidizes and becomes brittle. The discoloration on the inside is called sugaring - it means the weld will corrode in service.

A trader bought cheap heaters from a shop that brazed the end caps. They lasted 3 months in a water tank. We cut one open - the brass filler was porous and water had crept along the joint. TIG welded units run 5 years in the same tank.

Post-weld test

Every welded end goes into a water bath. We pressurize the tube with 0.5 MPa air and look for bubbles. If any bubble comes out, the weld is bad and gets re-done. No exceptions.

Need TIG-welded tubular heaters?

We TIG every end, purge on special alloys, and leak test before shipment.

Send Your Specs
Get a Quote