Incoloy 800 and 840 are the standard sheath materials for high temperature tubular heaters - up to 600 C in air. They weld differently from stainless.
Why Incoloy is tricky
Incoloy has high nickel and chromium. When you weld it without argon on the back side, the chromium oxidizes. The weld loses its corrosion resistance and becomes brittle. The technical term is intergranular oxidation - it looks like sugaring on the inside.
Welding procedure
- TIG only, with ERNiCr-3 filler (Inconel 82)
- Argon backing gas inside the tube during welding
- Clean the tube ends with stainless brush, no oil or grease
- Low heat input - 60 to 80 A, thin beads
- Interpass temperature under 150 C - do not let it get red hot
What bad Incoloy weld looks like
The outside weld looks fine. Cut it open and the inside is gray and oxidized. In service, that oxidized layer flakes off, the weld cracks, and the heater fails in months.
A customer bought Incoloy heaters from a cheap supplier. They looked the same but failed after 6 months in a 500 C oven. We sectioned one - the inside weld was sugared black. We provide argon backing on every Incoloy weld. Our units run 3+ years.
Need Incoloy high-temp heaters?
We back every Incoloy weld with argon. No sugaring, no early failure.