Brazing vs Welding for Heaters: When Silver Braze Is the Right Call

Not every joint on a heater needs full TIG welding. Some joints - like a thermocouple boss on a tube, or a terminal pin on a cartridge - are silver brazed. There is a time and place for each.

Welding (TIG)

Melts the base metal and filler together. Full penetration. Hermetic. Good for pressure boundaries and wet environments. Heat affected zone is large, can warp thin parts.

Brazing (silver alloy)

Heats the parts to 600 to 800 C, melts a silver-copper filler that flows into the gap by capillary action. Base metal does not melt. Lower heat, less distortion. But the joint is not as strong, and silver braze can corrode in certain acids.

Where we braze

Where we never braze

Any joint that touches liquid or holds pressure. Silver braze is porous over time in wet service. The end cap on an immersion heater must be TIG welded, never brazed.

A customer had a brazed flange joint leak after a year in a water tank. The silver braze had corroded. We replaced with TIG welded 316L. No leak since.

Need the right joint for your application?

We TIG pressure boundaries and braze non-critical joints. Tell us the service.

Send Your Specs
Get a Quote